Bonding the SNSPD

We bond directly to NbTiN, with the following parameters on the Bonding machine.

NbTiN, 10 nm on SiO2 (Based on Juliens notes)
Unclear parameters: Look: 3.0, Toil: 2.9, Tea: 3.0?

step 1 step 2
Search 1.09 1.13
Power 2.86 2.82
Time 3.0 3.0
Force 2.8 2.7